• TAPPI T813
Provide PDF Format

Learn More

TAPPI T813

  • Tensile Test for the Manufacturer's Joint of Fiberboard Shipping Containers
  • standard by Technical Association of the Pulp and Paper Industry, 12/01/2004
  • Publisher: TAPPI

$30.00$59.00


This method is used to determine the strength of the manufacturer's joint of commercially made corrugated and solid fiberboard shipping containers.It is applicable to taped, stitched, or glued joints and may also be used to evaluate laboratory fabricated joints similar to commercially made joints.