  • Wear Progress Of Vitrified Bonded Cbn Wheels
  • standard by Society of Manufacturing Engineers, 06/01/1995
  • Publisher: SME

$9.00$18.00


BY VITRIFIED BONDED CBN GRINDING WHEELS, THE EROSION OF THE BONDING MATRIX DOMINATES AS THE WEAR MECHANISM. GRINDING TESTS CONFIRM THAT THE LOAD FROM THE CONTACT ZONE IS AFFECTED BY THE GRINDING CHIPS. EMPIRICAL DATA DEMONSTRATES THAT USING THE SAME SPECIFICATIONS OF VITRIFIED BONDED, BUT DIFFERENTLY SIZED CBN WHEELS, THE GRINDING RATIO G CAN BE DRAWN AS A MATHEMATICAL FUNCTION OF A (subscript cu).

Related Products

SME MR98-251

SME MR98-251

Excimer Laser Micromachining Of Nylon..

$9.00 $18.00

SME MS00-230

SME MS00-230

Auto-Tuning Adaptive Supervisory Control Of Single-Plane Active Balancing Systems..

$9.00 $18.00

SME EM97-169

SME EM97-169

Press Requirements For Compression Mold..

$9.00 $18.00

SME MS910267

SME MS910267

Improving Quality And Productivity Through Filter Media Selection..

$9.00 $18.00