  • Development Of Guidelines To Prevent Internal Cracking During Induction
  • standard by Society of Manufacturing Engineers, 06/01/1995
  • Publisher: SME

$9.00$18.00


IN THIS STUDY, SEVERAL CASES OF INTERNAL CRACKS COLLECTED FROM VARIOUS FORGING COMPANIES WERE ANALYZED USING A FINITE ELEMENT APPROACH TO IDENTIFY THE CAUSES OF THIS PROBLEM. IT WAS FOUND THAT TWO OF THE MAIN CAUSES ARE: EXCESSIVE DEFORMATION DURING COLD FORGING, AND HIGH TENSILE THERMAL STRESSES DURING INDUCTION HEATING. GUIDELINES FOR PREVENTING INTERNAL CRACKING DURING INDUCTION HEATING WERE DEVELOPED ON THE BASIS OF THIS ANALYSIS.

Related Products

SME MS910465

SME MS910465

Flexible Manufacturing System Design And Operations Planning Using Simulation..

$9.00 $18.00

SME MS94-210

SME MS94-210

Simulation And Calibration For Off-Line Programming Of Industrial Robotsi..

$9.00 $18.00

SME AD98-170

SME AD98-170

Induction Brazing..

$9.00 $18.00

SME AD920205

SME AD920205

Emerging Technology For Large-Area Scanning Of Aging Aircraft..

$9.00 $18.00