Learn More

SAE AMS2759/1E

  • Heat Treatement of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa)
  • standard by SAE International, 02/06/2009
  • Publisher: SAE

$37.00$74.00


This specification, in conjunction with the general requirements for steel heat treatment covered in AMS 2759, establishes the requirements for heat treatment of carbon and low-alloy steel parts to minimum ultimate tensile strengths below 220 ksi (1517 MPa). Parts are defined in AMS 2759.

Related Products

SAE AS5716A

SAE AS5716A

Standard Electrical and Logical Interface for Airborne Fuzing Systems..

$37.00 $74.00

SAE AS1895/5C

SAE AS1895/5C

FLANGE, MALE, SEAM WELD, TYPE II LOW PROFILE..

$37.00 $74.00

SAE AMS5808C

SAE AMS5808C

Steel, Corrosion and Heat-Resistant, Welding Wire 19Cr - 13Ni - 2.5Mo High Ferrite Grade, Trace Elem..

$37.00 $74.00

SAE AS85049/148

SAE AS85049/148

INDIVIDUAL SHIELD TERMINATION, CONNECTOR, ELECTRICAL (CATEGORY 9)..

$37.00 $74.00